Cordierite
click:2276
belong to:Cordierite
Release time:2024-04-24 10:10:29
TEL:+0086-15037978556
Online Message
details
Items |
WJ |
BWJ |
GJ |
SiO2 (%) |
49-51 |
45-50 |
45-50 |
Fe2O3 (%) |
≤ 0.5 |
≤ 1.0 |
≤ 1.5 |
Al2O3 (%) |
34-37 |
35-38 |
35-38 |
MgO(%) |
13-15 |
11-15 |
11-15 |
Bulk Bensity ,B.D. g/cm³ |
≥1.65 |
≥ 1.7 |
≥ 2.0 |
Cordierite has very low thermal expansion and can promote thermal shock resistance, and can be applied in bricks and castables.